Woven nickel mesh (30-60 mesh, Ni201) is the right catalyst substrate. Knitted nickel mesh (660-850 g/m2, Ni201) is the right porous transport layer. Ni201 annealed wire is the right current collector. One material cannot cover all three positions, and in our post-mortems a stack failure rarely traces back to just one bad call anyway. Pick wrong at any position and that mistake sets the ceiling for the entire stack lifetime, no matter how good the catalyst, membrane or balance of plant is.

TL;DR: 3 positions, 3 materials: woven Ni201 mesh (catalyst substrate, 30-60 mesh), knitted Ni201 mesh (PTL, 660-850 g/m2, 90-95% porosity), Ni201 wire (current collector, annealed, 0.5-2.0 mm). Ni foam collapses under compression. SS 316L fails via SCC in hot KOH. Specify by position, not by product.

Three Electrode Positions, Three Material Requirements

1. Catalyst Support Substrate. This position needs three things at once. Uniform aperture distribution, so current density stays consistent. High surface adhesion, so the Raney nickel catalyst coating holds. And a burr-free surface finish, so the Zirfon or asbestos diaphragm never gets punctured mechanically. Recommended: woven nickel mesh, 30-60 mesh per inch, plain weave, 0.19-0.30 mm wire diameter, Ni201 grade, electropolished finish. Ordered aperture geometry matters here. Every unit cell of the electrode then carries the same electrical path length and the same catalyst loading. ASTM B456 and ISO 9044 compliant.

2. Porous Transport Layer (PTL). The PTL has to stay elastic. Stack clamping runs at 5-15 bar, and the layer must keep electrical contact through all of it. Volumetric porosity needs to sit above 85% so electrolyte and gas can move as a two-phase flow, and the material has to recover from repeated compression cycles across a 60,000+ hour stack lifetime. Recommended: knitted nickel mesh, 660-850 g/m2 packing density, single jersey knit, 90-95% porosity, Ni201 grade. The three-dimensional loop structure works like a spring. For large-area stacks above 1 m2 active area, where PTL collapse is the primary failure risk, use the interlock (double-knit) variant at 850-1150 g/m2.

3. Current Collector / Lead Wire. Here we look for 14-18% IACS conductivity to carry DC current from the busbar out to each electrode element, minimum 30% elongation so the wire can be formed and welded without trouble, and corrosion resistance that holds up in 30% KOH at 80-90 C. Recommended: nickel wire, Ni201 grade, annealed temper, 0.5-2.0 mm diameter for internal wiring. Carbon stays at 0.02% maximum in Ni201. That matters. In standard Ni200 (0.15% C), grain-boundary carbide precipitation (Ni3C) sets up intergranular corrosion after 20,000+ hours. ASTM B162 compliant.

Head-to-Head Comparison

CriterionWoven Ni MeshKnitted Ni MeshNi Foam (80-110 PPI)SS 316L
Porosity35-55% geometric85-98% volumetric85-98% volumetricN/A (solid plate)
CompressibilityRigidElastic spring-backPlastic collapseRigid
Current UniformityExcellent (ordered geometry)Good (elastic contact)Poor (random structure)Good (solid)
KOH Corrosion at 85 CPassive (stable Ni(OH)2 film)PassivePassiveSCC + Fe leaching into electrolyte
Dimensional StabilityExcellent (50,000+ hrs)Good under compressionPoor (pore collapse)Excellent
Industrial Track Record50,000+ hrs proven30,000+ hrs provenLab-scale onlyNot recommended for KOH
Cost (relative)$$$$$$$$
Best ForCatalyst substratePTL / spring layerR&D cells onlyExternal hardware only

Bottom line: Specify by position. The catalyst substrate, the PTL and the current collector are three different engineering problems. Woven Ni201 mesh, knitted Ni201 mesh and Ni201 wire together make up the matched electrode material set for alkaline electrolyzer stacks targeting 60,000+ hour lifetimes.

Frequently Asked Questions (FAQ)

Which material goes at each electrode position in an alkaline electrolyzer?

Woven Ni201 mesh (30-60 mesh, 0.19-0.30 mm wire, electropolished) as the catalyst support substrate, knitted Ni201 mesh (660-850 g/m², 90-95% porosity) as the porous transport layer, and Ni201 annealed wire (0.5-2.0 mm) as the current collector. No single material covers all three positions.

Why not use nickel foam or stainless steel electrodes?

Nickel foam collapses plastically under stack compression, and its random structure gives poor current uniformity, so it stays acceptable for R&D cells only. Stainless steel 316L loses passivation in hot KOH. Stress-corrosion cracking follows, and iron leaching poisons the catalyst. We recommend neither for stacks targeting 60,000+ hour lifetimes.

What specifications should an electrode material RFQ include?

Specify by position. Woven substrate at 30-60 mesh with 0.19-0.30 mm wire in Ni201 (ASTM B456, ISO 9044). Knitted PTL at 660-850 g/m² and 90-95% porosity, interlock above 1 m² active area. Ni201 annealed lead wire at 0.5-2.0 mm with minimum 30% elongation (ASTM B162).

Page last updated: 2026-09-02

Related articles

Need electrode mesh for your project?

Tell us your specification. Same-day technical quote with Mill Test Certificate sample.

Contact
Add RAS Thermal as a preferred source on Google